				Sand Mold question,
				Posted: Sun Jul 27, 2014 3:30 pm
				by jim burchett
				I have made a Box Sand Mold and have Pressed textures into the sand to make relief in the glass. I am wondering if I sift powders into the depressed areas of the mold and then take it to a Tack fuse temp if the powders will provide contrast to those areas?
			 
			
					
				Re: Sand Mold question,
				Posted: Sun Jul 27, 2014 4:26 pm
				by rosanna gusler
				Probably. The Fritz might ball up before the other glass touches dowm though
			 
			
					
				Re: Sand Mold question,
				Posted: Sun Jul 27, 2014 8:13 pm
				by jim burchett
				Well its worth a try...long slump at 1225 then quick up to 1400..will let you know how it works out.