Wax carbonisation temp?
Posted: Fri Aug 08, 2014 7:45 pm
Hello. Does anyone know at what temperature wax completely carbonises?
Pete
Pete
Guide to fusing, slumping, and related kilnforming techniques
https://warmglass.com/phpBB3/
You trying to burn wax and any organic contaminants completely out of the mold? That's around 800C.Peter Angel wrote:Hello. Does anyone know at what temperature wax completely carbonises?