Has anyone ever used bottom less slumping molds?
I am wondering how heat escapes from these bottomless molds that sit directly on the kiln shelf, and if there are any special firing considerations. I don't see anything on the seller's web site about needing to do anything special with these molds.
The only slumping molds I own all have heat escape holes in the bottom. I put these on short kiln posts when slumping. All very straightforward.
Thank You
Bottomless Molds - traditional slumping method?
Moderator: Tony Smith
-
Deive Butvila
- Posts: 22
- Joined: Sat Dec 21, 2013 10:39 am
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Bottomless Molds - traditional slumping method?
I'm guessing you're talking about Laurie Spray's molds. She will supply detailed firing schedules for you to start with. Most of her molds are fairly shallow; I've got one that I just use as I would any other. Many of my shallow molds don't have holes drilled in them anyway. But I'm a big advocate of 'low and slow' for my slumping.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Bottomless Molds - traditional slumping method?
We have been making our "Bottomless Molds" for almost 10 years now. They are fired just like you would any other slumping mold but you are guaranteed to always have a non rocking floor to your glass creation when using them. I got very tired of rocking bottoms on art pieces that were slumped onto molds that were basically made for the ceramic industry......and then just renamed glass slumping molds. We now make these molds from 4" to 18". Along with Valerie.....low and slow is the best way to slump.....but you can also slump and fire polish at the same time in low profile molds. Let us know if you have any questions.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Bottomless Molds - traditional slumping method?
The holes are to allow air to escape. Not heat. R.
artist, owner of wanchese art studio, marine finisher
-
Deive Butvila
- Posts: 22
- Joined: Sat Dec 21, 2013 10:39 am
Re: Bottomless Molds - traditional slumping method?
Yes, thank you for the correction.rosanna gusler wrote:The holes are to allow air to escape. Not heat. R.
-
Deive Butvila
- Posts: 22
- Joined: Sat Dec 21, 2013 10:39 am
Re: Bottomless Molds - traditional slumping method?
I guess I did not realize these are shallow low profile molds so not having vents makes some sense to me. I just have not had any experience with ventless molds.
Thanks to all for educating the newbie!
Thanks to all for educating the newbie!
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Bottomless Molds - traditional slumping method?
The fact that they have no bottom means that yes they are vented. Air can escape between the mold and the shelf. If it will not hold water it will not hold air. R.
artist, owner of wanchese art studio, marine finisher
Re: Bottomless Molds - traditional slumping method?
Just think of those center holes as great big vents... 
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)