Replacing common TC with Iconel- sheathed thermocouple

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Replacing common TC with Iconel- sheathed thermocouple

Post by Buttercup »

I'm about to replace the K type thermocouple in my brick kiln and have read everything I can find here on the WGB and see that Bert recommends an iconel-sheathed thermocouple and there don't seem to be any contraindications mentioned, so... will it just connect to the existing thermocouple leads to the sending unit or is it more complicated than that, please? This is the one I am thinking of getting:

http://www.tcdirect.net.au/deptprod.asp?deptid=190/2#1 Order code 608-410
Update:
The company tech just called me back and mentioned that the leads should not get hot. Maybe I'm better sticking to the old-type ceramic-cased thermocouple as there would probably be some heat transfer through the hole where the thermocouple is inserted through the brick, even if it is stuffed with insulation? He invited me to send him some pics, which I'll do if there isn't a python draped over the top of the kiln, as there was yesterday....bit of a shock after congratulating ourselves for snake-proofing the workshop!

Thanks, Jen
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Replacing common TC with Iconel- sheathed thermocouple

Post by Warren Weiss »

Jen,
Maybe you could use the python as a new thermocouple.
Warren
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Replacing common TC with Iconel- sheathed thermocouple

Post by Bert Weiss »

Jen, if that were the case, it would be impossible to use these thermocouples. I have used them for decades. Just hook the red wire and the yellow wire to the proper terminals and it works. I am told that the first couple of firings will be a bit off and then it will work well for a long time to come.

As to those first couple of firings, just do them. I wouldn't settle on schedules you use over and over until after that initial break in period is over.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Replacing common TC with Iconel- sheathed thermocouple

Post by Buttercup »

Warren, I discussed that with the python and apparently it's not on. There was some muttering about the comparative likelihood of inserting a marshmallow into a wildcat's a*%%. I'll follow Bert's advice first and revisit the python option if that doesn't work. He was assisted out of the workshop and a gap over the workshop door was closed. I hope he gets the message. I know I need recalibrating every time one appears. :shock:
Leaving the workshop
Leaving the workshop