fusing several large pieces together
Posted: Wed Oct 08, 2014 10:24 am
				
				I have a beautiful piece of dichroic irregularly shaped 1/8" 96 glass about 14"x8" that I want to fuse with a backing.  The first piece will be 1/8", and the other piece 1/4" ( or possibly one 1/4" and another 1/8" piece - I'd like to make the final product thick, and sturdy. ) 
I am worried about getting bubbles in the glass - a blow-out, which I've experienced on smaller pieces if ramping too quickly. Any suggestions on a good ramping time would be appreciated.
			I am worried about getting bubbles in the glass - a blow-out, which I've experienced on smaller pieces if ramping too quickly. Any suggestions on a good ramping time would be appreciated.