Page 1 of 1
MR97
Posted: Tue Dec 02, 2014 4:30 pm
by smallbitz
I have some older molds that I have used Slide on as a mold release. Do I need to sandblast them before I apply MR97, or can I put MR97 over the Slide? Anyone know?
Re: MR97
Posted: Tue Dec 02, 2014 5:16 pm
by JestersBaubles
My SWAG is that you can use it directly over the Slide. I would just brush off what I can of the slide and apply the MR-97.
I think you will like the MR-97 much better (I do).
Dana W.
Re: MR97
Posted: Tue Dec 02, 2014 8:26 pm
by smallbitz
Thanks. I've used MR97 for a while and like it much better then Slide, but haven't used it on these older molds, or over Slide before. Appreciate the info!
Re: MR97
Posted: Thu Dec 04, 2014 2:29 am
by Laurie Spray
Brush mr97 out after using and lightly mist.....and yes over slide.