I was looking at Bullseye reactive glass chart. I'm not sure I'm reading it correctly.
Can you get reactions from any of the transparent glasses? Most of those listed say "opal".
Thanks,
Vernelle
reading BE reactive chart
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: reading BE reactive chart
The chart is pretty clear..you get reactions from the glasses listed..if it says opal then opal is where the reaction is
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Re: reading BE reactive chart
Make sure you're looking at the latest version: http://www.bullseyeglass.com/images/sto ... _glass.pdf
The older versions used to list the transparent and opal glasses separately. The new chart mixes them up.
Opal glasses will have a 0 in the 4th from last position in the product number, as in "000208." Transparent glasses will have a 1 in that position, as in "001818."
The older versions used to list the transparent and opal glasses separately. The new chart mixes them up.
Opal glasses will have a 0 in the 4th from last position in the product number, as in "000208." Transparent glasses will have a 1 in that position, as in "001818."
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)