Page 1 of 1
My latest deep slump vessel
Posted: Fri Jan 02, 2015 4:36 am
by Babette (Shawn)
This piece was done with stringers and frit and one piece of steel blue sheet glass. If you look at the rim you can see the steel color.
Re: My latest deep slump vessel
Posted: Fri Jan 02, 2015 12:06 pm
by Warren Weiss
Babette,
That is a lovely bowl! How deep is it? Was it done in a single slump or using the "3 bowl" slump technique? Thanks.
Warren
Re: My latest deep slump vessel
Posted: Fri Jan 02, 2015 8:06 pm
by twin vision glass
Oh so fantastic and beautiful and well, totally inspiring! Les
Re: My latest deep slump vessel
Posted: Fri Jan 02, 2015 10:12 pm
by Babette (Shawn)
I used the deep slump bowl #2 and #3, I started with a 20 inch disc, slumped into my old stainless steel sink mold for the first slump so in total it was slumped 3 times. The finished bowl is 9 inches deep and an inch thick, lots of glass!
Re: My latest deep slump vessel
Posted: Fri Jan 02, 2015 10:47 pm
by Warren Weiss
Babette,
Thanks. That is quite a statement in glass. Worth every pound of it!
Warren
Re: My latest deep slump vessel
Posted: Sat Jan 03, 2015 3:03 am
by Buttercup
Well done, Shawn!
Re: My latest deep slump vessel
Posted: Mon Jan 05, 2015 8:04 am
by Lori Schinelli
very nice piece!