Casting and Annealing over 20cm/8in

Posted: Sat Jan 03, 2015 1:26 pm
by lucho/lachezar/
Hi all!

I'm about to cast a head with part of a chest where my thickest part is 23cm thick ...
Should I calculate a ratio based on the BE table (ending at 20cm) or are there any other ways?

Thanks!

Here are 2 pictures of the plaster model of the sculpture. It is a life size figure of a young boy - 1.55m tall. Most of it is to be bronze (already cast) and the head, the collar of the coat, the waistcoat and the shirt are going to be glass.

Lucho