Best COE red glass for high fire melts
Posted: Fri Feb 20, 2015 4:20 pm
by Lee Sorg
I'm new to the Warm Glass forum, so first, thanks for including me. I am doing high fire temparature melts and discovering that transparent red does not stay red once it reaches high temps of 1700 degrees. The red turns a muddy liver brown, kinda yucky looking. So my question is, what, if any, COE90 reds work well for high fire melts and pours? Thanks in advance for your answers.
Re: Best COE red glass for high fire melts
Posted: Fri Feb 20, 2015 6:03 pm
by Brad Walker
The transparents will usually turn opaque and ugly.
Of the opaques, 0024 Tomato Red seems to hold up best. The 0124 Red often reduces to brown.
Re: Best COE red glass for high fire melts
Posted: Fri Feb 20, 2015 6:50 pm
by Lee Sorg
Great. Thanks Brad.
Re: Best COE red glass for high fire melts
Posted: Sat Feb 21, 2015 1:41 am
by jim simmons
Can you try an oxidizing atmosphere?
Jim
Lee Sorg wrote:Great. Thanks Brad.
Re: Best COE red glass for high fire melts
Posted: Sat Feb 21, 2015 10:39 am
by Brad Walker
jim simmons wrote:Can you try an oxidizing atmosphere?
You could, but it's bad for the kiln elements.
Re: Best COE red glass for high fire melts
Posted: Sat Feb 21, 2015 1:44 pm
by Lee Sorg
Thanks for the suggestion Jim. I'm not sure how to oxidize the atmosphere in a kiln. But it sounds like this would not be a safe approach anyway. I did go ahead and order the 0024 Tomato Red — it looks like using this glass will work. After my first attempt using transparent red did not work out so well, I need a path that will yield a predictable result. Thanks again, all your feedback is much appreciated.
Re: Best COE red glass for high fire melts
Posted: Sat Feb 21, 2015 3:06 pm
by rosanna gusler
Brad Walker wrote:jim simmons wrote:Can you try an oxidizing atmosphere?
You could, but it's bad for the kiln elements.
Isn't it opposite of that? A reducing atmosphere will strip off the protective oxide coating that is on the elements.
Re: Best COE red glass for high fire melts
Posted: Sun Feb 22, 2015 5:02 pm
by Morganica
You have to move to casting glasses to find a red that will work in high fire melts. Look at Burnt Scarlet Striker--it holds up very well to the heat. It is not a pure fire-engine red, however--it's got a bit of an orangey cast and is a little dark in thick castings. In thinner applications, such as pot melts, it'll probably look fine.

Re: Best COE red glass for high fire melts
Posted: Mon Feb 23, 2015 8:02 pm
by Lee Sorg
Thanks Cynthia, I'll give the Burnt Scarlet Striker a try.