graphite

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

graphite

Post by mikefromitaly »

Hi.
i would like to know how to cut Grafite Plates.

thank you

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: graphite

Post by charlie »

you buy them. it depends upon how big you need. marble or bead makers use them. you can probably get them off ebay cheaply.
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: graphite

Post by Brad Walker »

mikefromitaly wrote:i would like to know how to cut Grafite Plates.
A diamond saw blade will cut graphite.
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: graphite

Post by The Hobbyist »

Graphite machines very nicely with nearly any cutting tool, even hand tools. The big problem is handling the shavings. When I work it I keep a vacuum constantly cleaning the cutting site so they don't fall or float about.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Sean McFeely
Posts: 3
Joined: Thu Jul 23, 2015 9:52 am

Re: graphite

Post by Sean McFeely »

I agree with the hobbyist. If you are not careful to manage the dust you can and will short out your bushings on your electric motors as the dust is a conductor.