French Cleats

Post by Cate G »

I saw the new video on the Bullseye site yesterday. Leslie from Twin Visions asked about where to get french cleats and the Dow 995 silicone. I found some french cleats in Home Depot, manufactured by OOK. They were in the isle with the picture hanging stuff and screws and nails and stuff. They were $7.97 for a 5" or 6" one (60 lbs), $9.97 for a 12" (100 lbs) and $14.97 for an 18" one ( 200 lbs). They looked like aluminum. The Dow they didn't have, so I guess online is the best place for that.
Just thought you might like to know...
Cate
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: French Cleats

Post by The Hobbyist »

Both can be found on p. 61 of the new Bullseye catalog.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Cate G
Posts: 65
Joined: Thu May 05, 2005 6:30 am
Location: Paramus, NJ and Parksville, NY
Contact:

Re: French Cleats

Post by Cate G »

That's good to know
Cate
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: French Cleats

Post by Valerie Adams »

I've been using Panel Clips for years, purchased through Brooklyn Hardware in Oregon. They're inexpensive and look like the ones in the Bullseye Catalog:
http://www.panelclip.com/our-products/
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: French Cleats

Post by DonMcClennen »

If you can't find the Dow product I always us GE Silicone II on french cleats with excellent results!
"The Glassman"
Cate G
Posts: 65
Joined: Thu May 05, 2005 6:30 am
Location: Paramus, NJ and Parksville, NY
Contact:

Re: French Cleats

Post by Cate G »

I have used that in the past,Don. I haven't made anything that was so large and heavy that I was worried about it falling off the wall.
Cate
smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: French Cleats

Post by smallbitz »

Don - How long do you let the GE Silione II cure before you feel safe hanging the piece?
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: French Cleats

Post by Bert Weiss »

smallbitz wrote:Don - How long do you let the GE Silione II cure before you feel safe hanging the piece?
72 hours is usually a safe curing time.
Bert