Its been sometime since I made a plaster mold and I cant remember what all goes into it.
Can someone please give me the recipe.
Thank you,
Andrea
making an investment
Moderators: Brad Walker, Tony Smith
making an investment

"C'est Moi (Its Me)"
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: making an investment
The classic recipe is 1/3 plaster, 1/3 silica, 1/3 water by weight. Proportions can be close to those ratios and still work. There are lots of other recipes.
Mix dry ingredients together first, then add to water.
Mix dry ingredients together first, then add to water.