Hello all,
I would like to fuse (sandwich) thin copper wire between 2 sheets of 3mm glass and then slump into a shallow platter shape.
This would be 2 firings.
Will then wire inside the glass slump together with the glass? Or will the glass and wire separate out during the slump?
Pete
Fusing wire between 2 sheets and then slumping
Moderators: Brad Walker, Tony Smith
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Fusing wire between 2 sheets and then slumping
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: Fusing wire between 2 sheets and then slumping
it will slump but not stretch. if the drop is too much and causes the glass to stretch, then the wires can be pulled to the surface or even out of the glass. the wires will act like a wire melt in that case.
-
Judith Andre
- Posts: 28
- Joined: Thu Mar 20, 2003 2:38 am
- Location: Lincoln, NE
Re: Fusing wire between 2 sheets and then slumping
In my experience, the glass will break because it moves, the wire does not.
Judith