Fire polishing sanded glass
Posted: Thu Feb 19, 2004 4:39 pm
I am new at this posting, so bear with me...
My question is about fire polishing - time and temperature - how much without changing the shape of my glass. I have tried several times, but I am not getting the full polish I want. Can someone give me a few pointers? My last firing I took the kiln up to 1300 degrees and held for 30 minutes - I am working with very small jewelry pieces that I have sanded and shaped with a med grit grinding wheel.
My question is about fire polishing - time and temperature - how much without changing the shape of my glass. I have tried several times, but I am not getting the full polish I want. Can someone give me a few pointers? My last firing I took the kiln up to 1300 degrees and held for 30 minutes - I am working with very small jewelry pieces that I have sanded and shaped with a med grit grinding wheel.