Bullseye schedules

Posted: Mon Aug 03, 2015 12:55 pm
by frizzygirl
Hi all,

I am going to have a go at fusing some coarse frit in Kaiser board molds to create pattern bars. My bars will end up 10cm x 4cm x 4cm. Is there a way I can calculate the fusing schedule for these size pieces as I will be firing 12 of them and don't want to mess it up. I have never done anything thicker than a 6mm platter.

I have looked at the Bullseye site but can't find an answer for this particular size. Is there a brilliant table like the potmelt one that calculates it once you enter the sizes.

Many thanks
Tracey

Re: Bullseye schedules

Posted: Tue Aug 04, 2015 6:37 pm
by Charlotte Kay
Have you seen this Bullseye tip sheet for thick slabs?
https://www.bullseyeglass.com/images/st ... _slabs.pdf