Patty Gray Mold
Moderators: Brad Walker, Tony Smith
Patty Gray Mold
I just purchased one of the Patty Gray Dam Mold. I kiln washed it and then found some instructions on the web that indicated to use boron nitrate. Is kiln washed and then lining with shelf paper ok to use?
Re: Patty Gray Mold
Boron nitrate ain't. You'll want boron nitride but if this is a ceramic mold then I don't know why kiln wash won't work. Lining with shelf paper before firing will most likely get you a lump of crumpled fiberpaper in the bottom of the mold, stuck to the glass in ways you won't like.
However, I haven't gone through the tutorial........
However, I haven't gone through the tutorial........
-
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Patty Gray Mold
Love the PG Dam molds. Use them per the directions and you will have good success. That being said, I think kiln wash would be fine, but do line the bottom with Papyros or Thinfire.
2 cents,
Dana W.
2 cents,
Dana W.
-
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Patty Gray Mold
Why not Ask Patty?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie