Posted: Fri Sep 18, 2015 6:37 am
by Maggie Abdel Rahman
Hi to all artists...
I am trying to figure out what kind of colors were used in the attached pictures : beautiul coral and violet transparent colors in Janet Kelman's seafans. I am currently using Provetro frit which gives me very nice colors, but shades are very dark in violet and orange.
I appreciate your opinion

Re: transparent fusing colors

Posted: Fri Sep 18, 2015 10:11 am
by DonMcClennen
I don't think it is appropriate to be posting photos of other peoples work! maybe that's why the photos are missing?

Re: transparent fusing colors

Posted: Fri Sep 18, 2015 12:58 pm
by Brad Walker
Maggie Abdel Rahman wrote:Hi to all artists...
I am trying to figure out what kind of colors were used in the attached pictures : beautiul coral and violet transparent colors in Janet Kelman's seafans. I am currently using Provetro frit which gives me very nice colors, but shades are very dark in violet and orange.
I appreciate your opinion
Janet Kelman's seafans use rondels that are made by a blower, not glass that is commercially available.

She discusses this on her website: http://janetkelman.com/

Re: transparent fusing colors

Posted: Fri Sep 18, 2015 8:09 pm
by Maggie Abdel Rahman
Thank you Brad