BE white 0113 in screen melt?

Post by Ann Fowler »

I saw a post on a glass forum on Facebook about a pot melt cracking because it had BE opaque white 013 in it. Does anyone know if the regular white, 113, is also dicey at high temps? Also, the scraps of 113 I want to use (in a screen melt) have an irid coating. I'm guessing the irid will burn off at screen melt temps, but otherwise, would there be any problem using it? Thanks in advance for any advice!
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: BE white 0113 in screen melt?

Post by The Hobbyist »

The irid does not burn off. It is metallic and in my experience it floats to the top.

Regular white tends to be wimpy in melts but does not cause cracking.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Ann Fowler
Posts: 2
Joined: Sun Sep 24, 2006 4:37 pm

Re: BE white 0113 in screen melt?

Post by Ann Fowler »

Thanks for the reply, Jim!