bubble in 10x10
Posted: Sun Nov 01, 2015 10:20 pm
				
				I do not like to use fibre paper, and put a 10x10 1/8" piece with fruit onto the kiln washed shelf.   I ran a program that was for fusing from Youghegheny, and the glass ended up with a big bubble in the almost center.   I've heard of putting small chips of glass in the four corners, to ease the glass down onto the shelf, and will try that.   Any other ideas would also be helpful.
The ramp was
Full fuse
300-800-10
300-1120-10
200-1250-10
500-1560-10
9999-1020-30
100-800-30
			The ramp was
Full fuse
300-800-10
300-1120-10
200-1250-10
500-1560-10
9999-1020-30
100-800-30