I wish to mount thick cast glass - like dalles, but glass cast and stained in my kilns, 15-25mm thick - in a resilient framework, able to withstand occasional vibration. The Liverpool Metropolitan Cathedral has its acres of glass set in a sort of black rubbery matrix, which would be perfect! But - what is it? It looks rather like the rubbery stuff that they lay down under the play equipment in children's playgrounds.
architectural glass mounting ... rubber/epoxy?
Moderators: Brad Walker, Tony Smith
-
- Posts: 23
- Joined: Thu Dec 16, 2004 5:59 pm
- Location: Liverpool UK
- Contact:
-
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: architectural glass mounting ... rubber/epoxy?
I'm thinking it might be a form of a material like Thiokol which is black and is/was used to install car windshields... flexible and very strong..
"The Glassman"
-
- Posts: 23
- Joined: Thu Dec 16, 2004 5:59 pm
- Location: Liverpool UK
- Contact:
Re: architectural glass mounting ... rubber/epoxy?
Thanks.... but no, this stuff is two-three inches deep, more like the dimensions of the concrete in modern architectural stained glass panels.
??? Tony
??? Tony
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: architectural glass mounting ... rubber/epoxy?
You can get silicone epoxy that comes in 2 parts. Some are clear and others not.
I am a fan of using L screws. They are minimally visible, and will not let the load fall off.
I am a fan of using L screws. They are minimally visible, and will not let the load fall off.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: architectural glass mounting ... rubber/epoxy?
You can get black flexible grout but that's assuming the glass is mounted to something I believe.