FTC Error Message on Paragon Kiln
Posted: Fri Nov 20, 2015 3:51 pm
				
				OK, this is more kiln related.
I tried calling Paragon, but they don't have business hours on Friday.
So, I programed and fired my school's kiln, a Paragon Dragon. I programed a 300 DPH cool down. I got the FTC message because the kiln naturally cools slower than 300 DPH.
OK, so my question.
We got the error message, but the kiln continued to cool down as per the program, or as closely as possible, right?
We fired pottery and glass, and the kiln had already gone through the anneal zone, but... I'm not sure. This is my students' stuff. I just need reassurance here.
Come on guys. Help a fellow artist out.
			I tried calling Paragon, but they don't have business hours on Friday.
So, I programed and fired my school's kiln, a Paragon Dragon. I programed a 300 DPH cool down. I got the FTC message because the kiln naturally cools slower than 300 DPH.
OK, so my question.
We got the error message, but the kiln continued to cool down as per the program, or as closely as possible, right?
We fired pottery and glass, and the kiln had already gone through the anneal zone, but... I'm not sure. This is my students' stuff. I just need reassurance here.
Come on guys. Help a fellow artist out.