SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
JoanG
Posts: 8
Joined: Tue Oct 12, 2004 8:39 pm

SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?

Post by JoanG »

I've been full fusing 7 inch plates for years, using the same schedule. I use a small hot start kiln that doesn't allow much in terms of controlling the heat, ramp speed, etc. I use a tiny amount of glue to hold the top and bottom pieces in place. Suddenly there are "bubbles" under the top layer and the glass isn't firing flat for the full fuse. I'm not sure how to attach a photo but any ideas or suggestions would be GREATLY appreciated! Thank you.
Attachments
Screen Shot 2015-11-28 at 5.03.39 PM.png
Screen Shot 2015-11-28 at 5.03.39 PM.png
Jordan Kube
Posts: 18
Joined: Sun Oct 01, 2006 10:40 pm
Location: Seattle

Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?

Post by Jordan Kube »

Perhaps you've lost an element or they are getting old, etc.
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?

Post by Brad Walker »

What schedule did you use? Is the top or bottom glass a different one that the one you've used in the past?

Does the kiln have top only elements or side and top?
Emily Speight
Posts: 11
Joined: Sat Dec 17, 2011 3:07 pm

Re: SUDDENLY ...air bubbles..SUGGESTIONS PLEASE?

Post by Emily Speight »

is there any possibility that your shelf has a small dip in it? perhaps you were using one side and flipped it?

while it's a workaround, a very fine sifting of clear powder between the layers can help prevent bubbles.

i would like to see your schedule...