Page 1 of 1
Vermiculite board
Posted: Sun Dec 20, 2015 2:13 pm
by Chris Lowry
So I carved out a vermiculite board to make a slumping mold... Do I need to put kiln wash on it before slumping?
I think no but the wife doesn't agree with me and now I'm doubting myself.
Re: Vermiculite board
Posted: Sun Dec 20, 2015 2:58 pm
by Bert Weiss
Chris Lowry wrote:So I carved out a vermiculite board to make a slumping mold... Do I need to put kiln wash on it before slumping?
I think no but the wife doesn't agree with me and now I'm doubting myself.
Yes! a generous coating. V board has a wicked tendency to stick to glass when both are hot.
Re: Vermiculite board
Posted: Sun Dec 20, 2015 3:18 pm
by Chris Lowry
Thanks, I guess you should never doubt the wife.
Re: Vermiculite board
Posted: Tue Mar 13, 2018 8:41 pm
by Ed Cantarella
Chris Lowry wrote:Thanks, I guess you should never doubt the wife.
Hey, she doubted you FIRST.