Page 1 of 1
Best Glue for Garden Stakes
Posted: Fri Mar 25, 2016 10:45 am
by grammy
I am replacing some glass for a client in their garden stakes. So these will be outside. The stakes do not have a way to "clip" in the glass, only glueing to the metal. What glue would be best? E6000?
Re: Best Glue for Garden Stakes
Posted: Fri Mar 25, 2016 3:26 pm
by Dick
I don't trust e6000 as I have had some failures. Loctite h30cl hysol works great and stays crystal clear.
Re: Best Glue for Garden Stakes
Posted: Fri Mar 25, 2016 9:43 pm
by grammy
Thank you.
Re: Best Glue for Garden Stakes
Posted: Sat Mar 26, 2016 4:55 pm
by DonMcClennen
GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
Re: Best Glue for Garden Stakes
Posted: Sun Mar 27, 2016 3:13 pm
by Valerie Adams
I'm with Don; silicone is my choice for outdoors.
Re: Best Glue for Garden Stakes
Posted: Mon Mar 28, 2016 8:05 pm
by grammy
Thanks. I did not find the Loctite that was mentioned but got an epoxy for metal to glass.
Re: Best Glue for Garden Stakes
Posted: Wed Apr 06, 2016 5:31 am
by Peter Angel
DonMcClennen wrote:GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
Don, do you ever get mold growing on the cured silicone?
Pete
Re: Best Glue for Garden Stakes
Posted: Thu Apr 07, 2016 8:06 pm
by Buttercup
Guess you can't replace it with grout, as we now have to do at all the floor/wall junctions in the showers. Damn! Jen