Devit Spray and Dichoric

Post by grammy »

I am making projects that seem to be getting devit on the second firing. These pieces will have dichroic on the top and tack fused. Will the clear coating affect the dichroic? TIA
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: Devit Spray and Dichoric

Post by Marian »

Yes, it is likely. Better to make a test strip with materials you intend to use. Devit spray can be blotchy or change the color of the dichroic.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Devit Spray and Dichoric

Post by Barry Kaiser »

There is devit spray, and there is devit spray.
Glass based devit sprays may well cause problems with dichro. I don't use them, so I can't say.
But borax based devit sprays do not affect dichro. Plenty of experience with that.
I have a tutorial on my web site on how to make cheap borax based agent.

Barry
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Devit Spray and Dichoric

Post by Judd »

My experience is that Homemade Anti-Devit spray removed iridized surfaces from fusible glass - but I've not tried it on dichroic. Good luck and post pictures please.
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Devit Spray and Dichoric

Post by grammy »

Thanks for the reply. I am going to try it later. My art show is over and I am going to relax for a little.