Page 1 of 1
					
				How to adhere stand up project to a glass base
				Posted: Wed Aug 17, 2016 8:41 am
				by LCS
				What is the best method and glue to adhere a stand up glass project to a glass base?
			 
			
					
				Re: How to adhere stand up project to a glass base
				Posted: Wed Aug 17, 2016 3:13 pm
				by JestersBaubles
				Depends upon the shape of the glass you are gluing to the base. If it has some means of support in its inherent design, you could use something as simple as E6000. I recently wrote a blog post on a candle shield, that might be helpful:
http://jestersbaubles.blogspot.com/2016 ... hield.html
If the glass piece can't support itself very well against gravity  

 I would use something like HXTAL.
Dana W.
 
			
					
				Re: How to adhere stand up project to a glass base
				Posted: Wed Aug 17, 2016 4:34 pm
				by DonMcClennen
				Glass to glass.. use UV adhesive