BE 1411, anyone knows????

Post by Havi »

Hello good friends,

Lately I bought some glass sheets, from someone who closed his workshop, .
Among them BUllseye 1411 - which looks reddish.
It does not appear on the online catalog, and/ or the written catalog of BE. But it HAS a BE label on it!

Can anyone tell me what it is?

Many thanks in advance,
Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: BE 1411, anyone knows????

Post by Brad Walker »

Deep Plum Transparent: http://shop.bullseyeglass.com/catalog/p ... 8/id/1411/

Not sure if it's the same as 1105, which has the same name.

You might want to ask Bullseye for clarification.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: BE 1411, anyone knows????

Post by Havi »

Many thanks, Brad!



Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: BE 1411, anyone knows????

Post by The Hobbyist »

It was my mother's favorite color. It went out of production years ago but I made it my quest to acquire a bunch. She's passed and I still have a lot left, mostly thin and a couple halfs with irid.

It's a luscious deep pink/purple/plum. It is very close to Cranberry Pink 1311. It too was a striker and the cold sheet can vary considerably before firing. I've made a couple awesome square dishes using homemade 1411 frit and 1821 Erbium Pink frit.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: BE 1411, anyone knows????

Post by Havi »

Many thanks!
The glass I bought is 1.5 millimeter, few sheets of it.
We'll see what happens with it.


There is another 'something' red that I bought which is not on the catalog - but this one I do not recall the number.

I'll post a question later.
Thanks again, you are the best!

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: BE 1411, anyone knows????

Post by DonMcClennen »

I still have some 1311 and 1411 on my shelf... both were very $$ glass.. beautiful when fired! Don't waste it!!
"The Glassman"
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: BE 1411, anyone knows????

Post by Havi »

OK,
Thanks Don



Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Post Reply