Bottle Slumping: Labels on gift shop item had hard gloss on top of paper lables?

Post by BillsBayou »

I was in a gift shop recently and happened upon slumped bottles that had paper labels under a hard gloss coating. What is this coating?

The coating felt enough like glass to have me scratching my head. Further, I could not detect an edge seam to the coating. Either it feather's out nicely, or the entire bottle is coated.

My friends threw out the empty bottle of Dom Perignon from their wedding reception. I snagged it and would like to slump something nice for them. If I had a way of re-using the label, that'd be great.
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Bottle Slumping: Labels on gift shop item had hard gloss on top of paper lables?

Post by Brad Walker »

Probably a resin. It's a liquid that settles out and dries to a hard coating.

Most craft stores carry them.