squares iout of circles

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

squares iout of circles

Post by jim simmons »

I have a bunch of cut circles and would like o know how to calculate the maximum square in a given circle.
Any suggestions?
Thanks
The other Jim
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: squares iout of circles

Post by Barry Kaiser »

Back to basic geometry!
D squared divided by 2 equals S squared.

Where D is the diameter of the circle and S is the side of the maximum square.
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: squares iout of circles

Post by Tony Smith »

Jim,

Its 0.707 x diameter

So if you have a 10" diameter, 10" is the hypotenuse or long side of the square
Pythagorean theorem says the square of the hypotenuse of a right triangle equals the sum of the squares of the other sides so,
a^2 + b^2 = c^2
c=10, so 10 ^2 = 100
Since a square has equal sides, a = b so we can write the equation as
2 a^2 = 100
Dividing both sides by 2 we get
a^2 = 50
Take the square root of both sides giving you
a = sqrt 50 = 7.07
So for a 10" diameter, you can fit a 7.07" square. For any other diameter, you can just multiply 0.707 x diameter

I hope this helps

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: squares iout of circles

Post by Kevin Midgley »

.....and then after all those careful calculations there is the flow of the glass to consider.
AndyT
Posts: 170
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: squares iout of circles

Post by AndyT »

I just divide the circle in half both ways and then connect the ends of each line to the one next to it.
Post Reply