Page 1 of 1
Tack fusing, but different
Posted: Tue Oct 03, 2017 5:11 am
by Jan de Jong
Hello, I did a full fuse with 2 layers Spectrum glass. After that full fuse I did a tack fuse with 2 layers on the first glass. Temp. 750 degrees Celsius. But the 2 layers had spread out, it look like a full fuse. Do you have to use a lower temp. by 4 layers ? Jan de Jong
Re: Tack fusing, but different
Posted: Tue Oct 03, 2017 11:15 am
by Jan de Jong
Sorry, perhaps placed in the wrong topic. Jan
Re: Tack fusing, but different
Posted: Thu Oct 05, 2017 10:01 am
by Judd
No, posting here is fine.
How long did you hold at 750?
Re: Tack fusing, but different
Posted: Thu Oct 05, 2017 11:10 am
by Jan de Jong
Judd wrote:No, posting here is fine.
How long did you hold at 750?
For 10 minutes. Jan
Re: Tack fusing, but different
Posted: Fri Oct 06, 2017 9:11 am
by Judd
Are you sure your thermocouple is reading correctly?
Whatever the case, maybe hit your target temp for only 5 minutes?