Cheap vases - are they safe to fire?

Post by FusedLightStudio »

I bought some colored vases and bottles at Dollar Tree thinking that I could use them for color accents on my float glass creations. But when I broke them up, I saw that the thick bottoms are clear glass; only the thin sides have color.

I'm concerned that the colors are some superficial coating (like lead-based paint?!) that will give off toxic fumes when fired.

Anyone have knowledge or experience about this?
Lisa Schnellinger
Atlanta, GA
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Cheap vases - are they safe to fire?

Post by Marty »

I'd be more concerned with incompatibility.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Cheap vases - are they safe to fire?

Post by Brad Walker »

Most likely the color will just go away in the firing. I've fired bottles that are similar and they just emerge from the kiln all clear.

I wouldn't worry about toxic fumes. And Marty's right -- the vase is probably not compatible with your normal float glass.
FusedLightStudio
Posts: 58
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Re: Cheap vases - are they safe to fire?

Post by FusedLightStudio »

Thanks very much, Marty and Brad. I’ll continue my experimentation with these limitations in mind!