Page 1 of 1

paragon window

Posted: Wed Apr 25, 2018 5:38 am
by mikefromitaly
Hello friends,

during a fusing the window of my paragin sc2 with door and window become black and i am not able to see inside anymore?

what do you think happened?..and any way to restore the glass to look again inside?

thanks for support and collaboration,

mike

Re: paragon window

Posted: Fri Apr 27, 2018 3:15 pm
by Joyce Walters
Hi Mike.
Do you know what caught on fire in the kiln?
Maybe it was just smoke from the kiln paper not vented?
Joyce from MT

Re: paragon window

Posted: Mon Apr 30, 2018 11:54 am
by Ed Cantarella
After trying to clean it, maybe try a little cerium oxide with a wet cloth. To polish the surface. Hopefully it is not ruined. :cry:

Re: paragon window

Posted: Mon Apr 30, 2018 2:22 pm
by mikefromitaly
Hi
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike