Potmelt from transparent glass
Hello ! Is it possible to do a potmelt with only transparant glass colours ? I did try it once.....all colours became dark ? Thank you ! Jan
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Potmelt from transparent glass
You will need to have your pot filled with at least 50% clear plus stick with lighter shades of transparent glass!
"The Glassman"
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Potmelt from transparent glass
Avoid reds, and pay attention to not mix reactive colors (or at least separate them from each other with a layer of clear).
Dana
Dana
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Potmelt from transparent glass
Thank you both for your answer ! I will try again. Jan de Jong
Re: Potmelt from transparent glass
In addition to reds...orange and yellow transparents will have a tendency to opalize at pot melt temperatures. So, unless you’d like this effect, you should avoid these colors.
Sharol
Sharol
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Potmelt from transparent glass
Thank you Sharol ! Jan