Page 1 of 1

glass sifters

Posted: Sat Mar 16, 2019 9:30 pm
by jim simmons
Anyone have any ideas as to what to use for sifting BE fine frit?
Not powder

Thanks in advance
The Other Jim

Re: glass sifters

Posted: Sun Mar 17, 2019 7:57 am
by Marty
To sort or to distribute? I'd start with a grading sieve. More distance from the work will give evenosity ™ (Brian B).

Re: glass sifters

Posted: Sun Mar 17, 2019 11:51 am
by jim simmons
Thanks, Marty It would be to distribute.
The other Jim

Re: glass sifters

Posted: Tue Mar 19, 2019 12:23 pm
by AndyT
jim simmons wrote:Anyone have any ideas as to what to use for sifting BE fine frit?
Not powder

Thanks in advance
The Other Jim
I've used a fine mesh tea ball/strainer.