Hello dear friends!
A while ago I was doing a mesh melt. Went as high as 1700F. I stayed there a bit more than recommended, as I wanted maximum glass to flow thru the mesh.
Was watching the kiln every once in a while - and it seemed to be working OK.
Then, about 5-6 hours after I started the firing, before going to bed for the night [probably after the annealing, ] I checked on the kiln, and was shocked to see that it stopped working!!!
It showed some strange remark , which upon checking in the manual - I learnt that it meant 'administrative warning' - or similar.
I was scared to hell, could not call anybody here [Israel] it was too late at night. Then called an American friend in USA , whose knowledge and experience I appreciate a lot.
He told me to shut the kiln off, and even unplug it - to make sure that it will not re-start . Wait until the morning, when the kiln cools down, and see what happened. It was a good advise. [MANY THANKS, B.!]
Luckily enough, the piece was done already, and it seems to me that the controller stopped working when upon going down at a rate of 180 degrees F [100 metrical].
My question is - Is typical to Orton in general,[I am sure it was AFTER annealing, as it looks OK], or is this my private controller ?
I would appreciate your comments and experience.
Many thanks,
Havi
My Orton controller - did it go wrong??
Moderators: Brad Walker, Tony Smith
My Orton controller - did it go wrong??
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: My Orton controller - did it go wrong??
What was the complete firing schedule?
Do you recall the exact error message?
Do you recall the exact error message?
Re: My Orton controller - did it go wrong??
please read down bellow,
Thanks
Thanks
Last edited by Havi on Sat Jun 08, 2019 3:10 am, edited 1 time in total.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: My Orton controller - did it go wrong??
Please read down below,
Thanks
H.
Thanks
H.
Last edited by Havi on Sat Jun 08, 2019 3:11 am, edited 1 time in total.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: My Orton controller - did it go wrong??
Hi Brad
Thanks for responding.
I believed I followed Immermans' schedule with variation,
in metric -
275 538 30
full 927 75 [i.e. 1700F]
full 820 45
full 482 1:30
28 427
54 371
I believe the error message was PLOG 0010 - CONTROLLER STORAGE DEVICE FAULT.
CAN you tell what causes this error, how could I prevent / avoid such errors.
And of course many thanks for your help - your will and your knowledge.
Havi
ps
I used this high temp. for a bit longer, as to allow more glass to melt thru the holes of the mesh, and to enable it to flatten in 1 uniform flat surface.
H.
Thanks for responding.
I believed I followed Immermans' schedule with variation,
in metric -
275 538 30
full 927 75 [i.e. 1700F]
full 820 45
full 482 1:30
28 427
54 371
I believe the error message was PLOG 0010 - CONTROLLER STORAGE DEVICE FAULT.
CAN you tell what causes this error, how could I prevent / avoid such errors.
And of course many thanks for your help - your will and your knowledge.
Havi
ps
I used this high temp. for a bit longer, as to allow more glass to melt thru the holes of the mesh, and to enable it to flatten in 1 uniform flat surface.
H.
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: My Orton controller - did it go wrong??
PloG errors mean the controller has detected a problem. It can be a lot of things. Sometimes it's just a glitch caused by a power surge or something that's a one off thing. PLoG 011, 012, or 013 errors mean there's a problem with a thermocouple. I believe 010 is a generic catch all error message (but not 100% sure).
In any case, you can usually get rid of the error by just pushing ENTER on the controller. If that doesn't work, do a two button (or even three button) reset. They're described on Orton's website here: https://www.ortonceramic.com/custpage.c ... _id=173533 (look for the FAQs about PLoG errors).
You can also email Orton directly here: https://www.ortonceramic.com/Contact%5FUs/ Try Jim Baldwin or Donna Malloy from the list on that page.
I don't see any issues with the program you're using.
In any case, you can usually get rid of the error by just pushing ENTER on the controller. If that doesn't work, do a two button (or even three button) reset. They're described on Orton's website here: https://www.ortonceramic.com/custpage.c ... _id=173533 (look for the FAQs about PLoG errors).
You can also email Orton directly here: https://www.ortonceramic.com/Contact%5FUs/ Try Jim Baldwin or Donna Malloy from the list on that page.
I don't see any issues with the program you're using.
Re: My Orton controller - did it go wrong??
Many thanks, Brad
What I got from this WGBB, and its participants -YOU - among them, is enormous. I owe you a lot. And I am endlessly thankful.
I shall copy and save what you wrote here, especially whom to turn to, in case of another catastrophe..
Thanks also for approving my schedule - it is important to me, as I love doing melts.
All the very very best,
Havi
What I got from this WGBB, and its participants -YOU - among them, is enormous. I owe you a lot. And I am endlessly thankful.
I shall copy and save what you wrote here, especially whom to turn to, in case of another catastrophe..
Thanks also for approving my schedule - it is important to me, as I love doing melts.
All the very very best,
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com