fusing glass laminate powder
Wondering if glass laminate (Arco) can be used in fusing. A friend gave me many boxes of this substance (old) in many colors. Can't find anything online about it, except that manufactured laminated glass is used as safety glass. Makes me think it might be something plastic. Very fine powder - like talc. Thanks for any info.
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: fusing glass laminate powder
In general glass laminate is used to laminate two pieces of glass together (like a front windshield in a car). It's a kind of plastic film between the two and can't be fused in the kiln.