Page 1 of 1
					
				Float Safety?
				Posted: Tue Feb 24, 2004 12:23 pm
				by GatorGirl
				Safety Experts Anyone?
I´m just curious if float glass truely is safe to eat off of? Or who to contact to find out? I´ve looked in the archives and there seem to be those who say it´s safe and others who say beware.   I know that BE clear is lead free and safe to eat off of...or so I´ve been told.   Is float that different? .
Thanks,
Kim
			 
			
					
				
				Posted: Tue Feb 24, 2004 12:56 pm
				by Bert Weiss
				Regular float glass is safe to eat off.  The crystal clear and tinted floats are also good.  I don't know about lowE...
			 
			
					
				
				Posted: Tue Feb 24, 2004 1:37 pm
				by GatorGirl
				Thanks Bert.  I thought so.  I e-mailed Ferro about sandwiching some of their food safe enamels between float glass and the man I e-mailed panicked! He panicked so I panicked.
			 
			
					
				
				Posted: Tue Feb 24, 2004 3:44 pm
				by Bert Weiss
				GatorGirl wrote:Thanks Bert.  I thought so.  I e-mailed Ferro about sandwiching some of their food safe enamels between float glass and the man I e-mailed panicked! He panicked so I panicked.
Sandwiching is tricky.  My technique is to prefire the enamels.  I recently heard about a technique of mixing the enamel with methyl cellulose medium (Klyr Fire) and not prefiring.  I haven't tried this yet, myself. 
When you talk to Ferro, you might be interested in their china paints as well as glass enamels.  In Germany you can get the transparent glass colors that are not available to us in the USA.  They might work very well sandwiched.  Different colors will behave differently.  They are probably lead bearing, but once they are sandwiched, there are no more problems. I wish we could get these colors.  They are fabulous looking.  Be sure to put both air sides of the float glass in contact with the enamels.  I would not fire hotter than 1420ºF to fuse the layers together. Soak for an hour somewhere around 1100 - 1220ºF  on the ramp up.
 
			
					
				
				Posted: Wed Feb 25, 2004 4:31 am
				by GatorGirl
				Thanks Bert for all of the info.  Do you know why they don´t sell the transparents to the US? I plan on visiting Frankfurt in a few weeks I guess I could ask them then.   I guess that is where their main headquarters are.  (By the way I loved your table top that you made by sand casting... using a jar lid for the texture!) 
Kim