Has anyone tried doing a pot melt onto fiber paper or Thin Fire?
Thanks
Michael
-
charlie
- Posts: 961
- Joined: Mon Mar 10, 2003 3:08 pm
Post
by charlie »
yes. don't. it will pull up fibers or dust into the glass, cause ugliness at the best, and incompatibilities and cracking at the worst.
i use a piece of glass for the melt to land on, and very fine layer of baby talc under that to allow the glass to slide without sticking.
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada
Post
by Tyler Frisby »
Any problems trying a Pot melt into a plaster/silica mold ? Ive thought It would be really swank to try

tanks a Milly