Soft fuse with flow?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Soft fuse with flow?

Post by Mark Wright »

Looking for help on how to achieve the texture in this picture from Pinterest. So far, I have not been able to reproduce it.
Textured fuse.jpg
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: Soft fuse with flow?

Post by Michael Stevens »

Contour fuse should do it. maybe. somewhere between tack fuse and contour fuse temps. the trick is to layer the glass long to short. I use a SS cake pan to. hold the shape while I'm forming.
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Re: Soft fuse with flow?

Post by Mark Wright »

Thanks for the hints. Based on your comment of using a cake pan it appears it also needs to be dammed. I'll give it a try.
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: Soft fuse with flow?

Post by Michael Stevens »

I use the cake pan to create the shape, don't need to cook it in that pan if you want organic and varied length. but I prefer even edge, I line the pan with kiln paper
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Soft fuse with flow?

Post by Don Burt »

are those edges of strips or stringers?
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Soft fuse with flow?

Post by Marty »

Don- it's strips on edge, cut in different widths so some will flop and flow. Watching the kiln is crucial until you know what happens when- you want the stuff stuck firmly to itself and the edges rounded nicely.