Heat resistant Tape

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Heat resistant Tape

Post by Jan de Jong »

Hallo, did see on a site heatresistant tape which was used by fusing. I marked the site as Favorite to look on it later.
Something went wrong.....no favorite and no idea where to search.
So my question is: is there tape with which you can fuse ?
Jan
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Heat resistant Tape

Post by Brad Walker »

So what are you wanting the tape to do?
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Heat resistant Tape

Post by Jan de Jong »

@ Brad Walker: Instead of Ceramic felt between RVS and the glass. I saw somebody use it on Internet. For Full fuse . Jan
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Heat resistant Tape

Post by Brad Walker »

That makes sense, just not sure why it would be better than fiber paper.

Most high temperature tape that I'm aware of is only rated to 500F, but might hold up longer insulated by glass. Google high temperature tape.
Post Reply