Just did my first simple frit piece-looked in the archives and used some hairspray, now question, do I tack it first or put a clear cap on it and full fuse-I could not find an answer in the archives. thanks Gayle

Posted: Tue Feb 24, 2004 11:18 pm
by Susan Moore
Gayle,

You can do either. It depends what look you want and since you are new to this you may as well do up some small samples - do some of each using different size frit, different colours, full fuse, tack fuse, etc.