Adjust firing schedule after multiple firings?
Posted: Thu May 27, 2021 11:07 pm
				
				I'm using COE96. I'm going to be working on a project that may require up to 4 firings. I'm testing some small tiles and after the 3rd firing, I'm seeing some slight incompatibility between Oceanside clear, bronze, and light amber. I have not changed the firing schedule for any of the firings. 
Do I need to adjust the schedule after the 2nd or 3rd firing or is this something that just happens to some colors?
Thanks for any information
Molly
			Do I need to adjust the schedule after the 2nd or 3rd firing or is this something that just happens to some colors?
Thanks for any information