Silver Fuming
I have made pieces in the past with Silver foil on BE reactive Ice and gotten a nice fume pattern. I am wondering if I use Tekta and Reactive Ice powder with Silver it will give a similar effect?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Silver Fuming
Silver needs to be on top for best results, but would work.
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Silver Fuming
Thanks, I always put the silver on top, I will run a cpl of text tiles tonight.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Silver Fuming
Test me the results.jim burchett wrote:text tiles
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Silver Fuming
While it did react, and there was some Halo, it wasn't nearly as intense as on the glass itself. Tried several different thicknesses of the powder, but it distorted the transparency in relation to its depth. So, these will just cost more in the future. So the answer is Yes, but....
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Silver Fuming
Maybe try to fuse the powder first then refuse with the silver?
The oher Jim
The oher Jim
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Silver Fuming
Too many steps then