Marking molds with ceramic pencil: Risk?
Posted: Wed Oct 20, 2021 10:46 am
				
				I took a mold to a nearby studio where other people work. It was there for a long time (studio had closed for COVID in the meantime). I found out that other people had been using It before I picked it up. 
I'd like to write on 'please don't use without permission' or something along those lines on the top side so it's apparent to others, but don't want it to transfer to the glass. I normally use ceramic pencil to put my contact info on the bottom. Would that transfer? Would a regular pencil work?
			I'd like to write on 'please don't use without permission' or something along those lines on the top side so it's apparent to others, but don't want it to transfer to the glass. I normally use ceramic pencil to put my contact info on the bottom. Would that transfer? Would a regular pencil work?