Drop out firing schedule

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Doug Zawodny
Posts: 33
Joined: Wed Feb 28, 2007 8:30 pm
Location: Sacramento California

Drop out firing schedule

Post by Doug Zawodny »

First time trying a drop out. I have a 15 in x1/2 disk over a 8in hole. Any suggestions for a firing schedule. I’ll be watching the drop to stop at 8in.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Drop out firing schedule

Post by Brad Walker »

Hold at 1250 to 1300 until done.