Hi,
I am running out of COE 96 casting plates and cannot find anymore. Sadness.
My castings are 6 to 7 feet tall and about 1.5 thick with frit on the surface of the mold.
Thinking of fusing 8 layers of 5mm clear sheets together.
Is this crazy or worth a try?
Appreciate any thoughts or info your can share,
Thanks, Peter
Fusing 5mm clear sheets
Moderators: Brad Walker, Tony Smith
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Fusing 5mm clear sheets
Switch to Bullseye glass.
Yes you can fuse sheets together however inevitably there will be bits of 'stuff like studio dust' between the layers.
Yes you can fuse sheets together however inevitably there will be bits of 'stuff like studio dust' between the layers.
-
Terry Gallentine
- Posts: 195
- Joined: Mon Jul 19, 2004 2:08 pm
- Location: River Falls, WI
- Contact:
Re: Fusing 5mm clear sheets
Peter--Did you go ahead and experiment with fusing multiple layers of 5mm clear together? If you did, did you use the Oceanside 96 or did you use the Wissmach 96? I am thinking about trying out the Wissmach 96 and might be interested in putting together an order with someone else for some full sheets (32"x42").