Gloves
Gotta take Plavix for 90 days. Need recommendations for cut proof gloves. Thanks in advance.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Gloves
A pair of regular nitrile or latex gloves should work fine. Gardening gloves are too thick and the gloves made for kitchen workers stop knife cuts but not glass ones.
-
Eric Bloom
- Posts: 8
- Joined: Fri May 15, 2020 3:39 pm
Re: Gloves
Mine came from Home Depot, in the tools section. They're marked "Premium Defense." Thinner than gardening gloves. Much thicker than latex or medical gloves - I wouldn't expect these to provide any protection from glass as they're designed to block dirt, bacteria and viruses.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Gloves
ansell vitriflex but I don't think they are made any more