Fusion Shield Update?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Brent
Posts: 2
Joined: Mon Mar 10, 2003 3:44 pm
Location: Millersburg, Ohio
Contact:

Fusion Shield Update?

Post by Brent »

I checked into the Fusion Shield shelves when they were first introduced, and remember seeing here that there were problems with outgassing and bubbles. As reported here, they improved from the first versions. There hasn't been anything (positive or negative) about them that I could find in the archives for about a year, and was wondering how those of you who are using them like them?

Have they really gotten rid of the early problems? Has the price come down any? Does anyone sell them, or do you still have to purchase direct? Thanks!
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Unfortunately, they weren't able to work out all the kinks and they have decided not to market the shelves to glass artists. Last I spoke to them, they promised to let us know if they decide to reenter the market.

It's a shame, because this could have been a great product.
Brent
Posts: 2
Joined: Mon Mar 10, 2003 3:44 pm
Location: Millersburg, Ohio
Contact:

Post by Brent »

Bummer! Thanks for the info, though, Brad. I hadn't thought about them for almost a year, but last night as I stood outside in the cold scraping shelves, they popped into my mind... :D