Drop out temp
Moderators: Brad Walker, Tony Smith
-
- Posts: 34
- Joined: Wed Feb 28, 2007 8:30 pm
- Location: Sacramento California
Drop out temp
Those out there doing drop outs, what is your high temp?
-
- Site Admin
- Posts: 1536
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Drop out temp
1300F. Never higher than 1325. Hold until drop is done.
-
- Posts: 34
- Joined: Wed Feb 28, 2007 8:30 pm
- Location: Sacramento California
Re: Drop out temp
Thank you.